Required materials:

Fine sandpaper ( e.g. 220 grainsize)

Protective gloves

Glaze- finish

Paintbrush

Steelwool ( medium degree of hardness)

 
 

Step 1:

Wood surface needs to be dry, dirt- and fat- free. Whet the surface in the direction of grain and dust it.

 
 

Step 2:

Apply glaze- finish thinly and evenly on surface in grain direction and let dry.

 

 
 

Step 3:

Intermediate sanding with 220 grain, always in grain direction. Thoroughly remove the dust afterwards.

 

Step 4:

Apply second coat and let dry.

 
 

Step 5:

After- treatment of wood surface with steelwool ( medium degree of hardness) in the direction of texture for achieving silky lustre.